3D Battery AnimationnLixMn2-yO4 Cells - Secondary Performance

 
 
LiMn2O4 Secondary Performance

Results of cyclng a Li-nLiMn2O4 cell between 4.5 and 2.5 V at a rate of 20 µA/cm2. The capacity loss is about 0.003% per cycle.

 

 

 
 

Results of continued cycling at 100°C. The higher capacity loss is due to a recrystallization of the cathode.

 

 

 
 

Increasing crystallinity of the cathode with cycling leads to a gradual change in the discharge curve.

 

 